Reconstruction of a former office building with ribbed slabs
Cracks in areas of cement; cement thickness approx. 4cm.
Wedge expanding of the cracks, cleaning from dirt, filling the gaps with epoxy resin WEBAC® 4170 until complete saturation, to restore traction.